WWW Computer Program for Producing Unrounded and Rounded Design Values for MOR, UTS, and UCS

This program takes ASTM D1990 characteristic values for MOR and produces unrounded and rounded design values for Modulus of Rupture (MOR), Ultimate Tensile Strength (UTS) and Ultimate Compression Strength (UCS). Property reduction factors for softwoods were used.
Please enter the MOR SS Characteristic value in psi

Please enter the MOR No. 2 Characteristics value in psi

The following information is also available:

Download Fortran Source Code

For further information on this program for producing unrounded and rounded design values, contact James Evans or call him at (608) 231-9332.

For problems with this web page, please contact Vicki Herian or (608) 231-9236.

[Forest Service] [Forest Products Lab] [FPL Statistics Group] [ASTM Allowable Properties Page]