Abarema jupumba & 0.661
Acacia albida & 0.526
Acacia arabica & 0.708
Acacia auriculiformis & 0.501
Acacia catechu & 0.875
Acacia chundra & 0.976
Acacia confusa & 0.747
Acacia dealbata & 0.616
Acacia decurrens & 0.626
Acacia erioloba & 1.001
Acacia ferruginea & 0.876
Acacia galpinii & 0.626
Acacia gerrardi & 0.731
Acacia goetzei & 0.834
Acacia granulosa & 0.561
Acacia hockii & 0.501
Acacia karroo & 0.654
Acacia lakai & 0.975
Acacia lenticularis & 0.717
Acacia leucophloea & 0.725
Acacia macrothyrsa & 0.949
Acacia mearnsii & 0.583
Acacia mellifera & 0.898
Acacia modesta & 0.845
Acacia nigrescens & 0.911
Acacia nilotica & 0.779
Acacia pavonima & 0.668
Acacia pennatula & 0.960
Acacia planifrons & 0.581
Acacia polyacantha & 0.696
Acacia richii & 0.690
Acacia robusta & 0.693
Acacia senegal & 0.773
Acacia seyal & 0.626
Acacia sieberana & 0.561
Acacia suma & 0.764
Acacia tomentosa & 0.517
Acer davidii & 0.444
Acer decandrum & 0.679
Acer mandshuricum & 0.614
Acer mono & 0.616
Aceude candeia & 0.770
Acrocarpus fraxinifolius & 0.587
Acrodicridium spp. & 0.906
Acronychia pedunculata & 0.417
Adenanthera pavonina & 0.731
Adenostephanus organensis & 0.557
Adina fagifolia & 0.610
Adina microcephala & 0.751
Adina minutiflora & 0.850
Adina pilulifera & 0.917
Adinandra acutifolia & 0.639
Adinandra fragrans & 0.722
Aegele marmelos & 0.754
Aextoxicon punctatum & 0.470
Africana bingeria & 0.276
Afrocrania volkensii & 0.501
Afzelia bipindensis & 0.660
Afzelia cochinchinensis & 0.748
Afzelia pachyloba & 0.630
Afzelia spp. & 0.670
Aglaia andamancia & 0.713
Aglaia argentea & 0.658
Aglaia dasyclada & 0.600
Aglaia diffusa & 0.699
Aglaia edulis & 0.702
Aglaia gigantea & 0.657
Aglaia iloilo & 0.527
Aglaia llanosiana & 0.892
Aglaia maiae & 0.597
Aglaia odoratissima & 0.717
Aglaia polystachya & 0.632
Aglaia roxburghiana & 0.783
Aglaia sapindina & 0.658
Aidia micrantha & 0.629
Aidia ochroleuca & 0.780
Ailanthus altissima & 0.521
Ailanthus excelsa & 0.328
Ailanthus glandulosa & 0.507
Ailanthus grandis & 0.350
Ailanthus malabarica & 0.365
Alangium chinense & 0.492
Alangium longiflorum & 0.648
Alangium meyeri & 0.631
Albizia acle & 0.573
Albizia amara & 0.700
Albizia amara & 0.719
Albizia antunesiana & 0.552
Albizia aylmeri & 0.626
Albizia brevifolia & 0.757
Albizia caribaea & 0.660
Albizia chinensis & 0.297
Albizia glaberrima & 0.520
Albizia glabrescens & 0.488
Albizia grandibracteata & 0.398
Albizia guachapele & 0.560
Albizia gummifera & 0.510
Albizia julibrissin & 0.585
Albizia kalkora & 0.482
Albizia lucida & 0.571
Albizia moluccana & 0.380
Albizia odoratissima & 0.632
Albizia procera & 0.647
Albizia saman & 0.470
Albizia saman & 0.536
Albizia saponaria & 0.629
Albizia schimperiana & 0.488
Albizia stipulata & 0.380
Albizia tanganyicensis & 0.257
Albizia thompsoni & 0.597
Albizia zimmermannii & 0.757
Albizia zygia & 0.472
Alchornea hirtella & 0.501
Alcornea latifolia & 0.490
Alcornea spp. & 0.385
Alcornea triplinervis & 0.365
Aleurites moluccana & 0.336
Aleurites moluccana & 0.389
Aleurites montana & 0.321
Aleurites trisperma & 0.427
Alexa grandiflora & 0.738
Allanblackia floribunda & 0.807
Allanblackia stanerana & 0.561
Allanblackia stuhlmannii & 0.565
Allophylus abyssinicus & 0.501
Allophylus africanus & 0.450
Allophylus chirindensis & 0.539
Alniphyllum fortunei & 0.388
Alnus ferruginea & 0.380
Alnus glutinosa & 0.446
Alnus japonica & 0.430
Alnus jorullensis & 0.380
Alnus nepalensis & 0.365
Alnus sibirica & 0.455
Alnus trabeculate & 0.437
Alphitonia neo-caledonica & 0.561
Alphitonia philippinensis & 0.395
Alphitonia zizyphoides & 0.500
Alphonsea arborea & 0.691
Alseia yucatanensis & 0.635
Alseodaphne hainanensis & 0.578
Alseodaphne insignis & 0.580
Alseodaphne longipes & 0.486
Alseodaphne semecarpifolia & 0.719
Alseodaphne umbaliflora & 0.520
Alstonia gilletii & 0.356
Altingia chinensis & 0.652
Altingia excelsa & 0.739
Altingia obovata & 0.723
Altingia yunnanensis & 0.613
Amblygonocarpus andongensis & 0.834
Amblygonocarpus obtusangulus & 0.829
Amburana acreanea & 0.498
Amburana cearensis & 0.498
Amesiodendron chniense & 0.803
Amomis caryophyllata & 0.821
Amomyrtus luma & 1.050
Amoora aherniana & 0.584
Amoora cucullata & 0.555
Amoora macrocarpa & 0.545
Amoora rohituka & 0.576
Amoora rugbiginosa & 0.700
Amoora wallichii & 0.496
Amphimas ferrugineus & 0.630
Amphimas pterocarpoides & 0.726
Amphimas spp. & 0.620
Anacardium giganteum & 0.493
Anacardium rhinocarpus & 0.507
Anacardium spruceanum & 0.420
Anacolosa densiflora & 0.781
Anadenanthera macrocarpa & 0.977
Anadenanthera rigida & 0.630
Angelesia splendens & 0.513
Aniba amazonica & 0.560
Aniba canelilla & 0.920
Aniba jenmani & 0.488
Aniba ovalifolia & 0.501
Aniba panurensis & 0.526
Aniba perutilis & 0.500
Aniba riparia & 0.620
Aningeria adolfi-friederici & 0.446
Aningeria altissima & 0.474
Anisophyllea obtusifolia & 0.630
Anisophyllea zeylanica & 0.460
Anisoptera aurea & 0.532
Anisoptera brunnea & 0.540
Anisoptera costata & 0.610
Anisoptera glabra & 0.475
Anisoptera grossivenia & 0.730
Anisoptera laevis & 0.490
Anisoptera marginata & 0.565
Anisoptera oblonga & 0.516
Anisoptera scaphula & 0.477
Anisoptera thurifera & 0.532
Anneslea fragrens & 0.557
Annona squamosa & 0.603
Annonidium mannii & 0.290
Anogeissus acuminata & 0.739
Anogeissus latifolia & 0.828
Anogeissus leiocarpus & 0.820
Anogeissus pendula & 0.795
Anogeissus phillyreaefolia & 0.719
Anogeissus sericea & 0.738
Anopyxis klaineana & 0.888
Anthocephalus cadamba & 0.435
Anthocephalus chinensis & 0.308
Anthocleista grandiflora & 0.603
Anthocleista keniensis & 0.500
Anthonotha macrophylla & 0.780
Anthostemma aubryanum & 0.320
Antiaris africana & 0.380
Antiaris spp. & 0.380
Antiaris toxicana & 0.358
Antiaris toxicaria & 0.372
Antiaris welwitschii & 0.449
Antidesma pleuricum & 0.593
Antidesma venosum & 0.578
Antrocaryon klaineanum & 0.500
Antrocaryon micraster & 0.479
Antrocaryon nannanii & 0.446
Aparisthmium cordatum & 0.488
Apeiba aspera & 0.280
Apeiba echinata & 0.360
Apeiba membranacea & 0.270
Apeiba spp. & 0.200
Apeiba tibourbou & 0.166
Aphanamixis cumingiana & 0.581
Aphanamixis perrottetiana & 0.511
Aphanamixis polystachya & 0.576
Aphananthe aspera & 0.525
Aphananthe philippinensis & 0.446
Aphloia theiformis & 0.526
Apodocephala pauciflora & 0.501
Apodytes dimidiata & 0.696
Apollonias canariensis & 0.671
Apollonias velutina & 0.671
Apuleia ferrea & 0.813
Apuleia leiocarpa & 0.772
Apuleia molaris & 0.760
Apuleia polygama & 0.770
Apuleia praecox & 0.719
Aquilaria agallocha & 0.347
Aquilaria sinensis & 0.375
Arbutus canariensis & 0.561
Archidendron oblongum & 0.356
Ardisia cubana & 0.620
Ardisia densilepidotula & 0.648
Artocarpus altilis & 0.270
Artocarpus altilis & 0.339
Artocarpus blancoi & 0.422
Artocarpus chaplasha & 0.424
Artocarpus comunis & 0.700
Artocarpus elasticus & 0.440
Artocarpus heterophyllus & 0.505
Artocarpus hirsuta & 0.516
Artocarpus integrifolia & 0.531
Artocarpus lakoocha & 0.530
Artocarpus lanceifolius & 0.620
Artocarpus nobilis & 0.629
Artocarpus ovata & 0.470
Artocarpus rigidus & 0.480
Artocarpus scortechinii & 0.430
Artocarpus styracifolius & 0.522
Artocarpus tonkinensis & 0.547
Arytera littoralis & 0.733
Assa leitao & 0.642
Asteropeia rhopaloides & 0.696
Astrocadrus chilesis & 0.365
Astronium balansae & 0.876
Astronium gracile & 0.730
Astronium lecointei & 0.743
Astronium macrocalyx & 0.976
Astronium ulei & 0.710
Astronium urundeuva & 0.925
Atalantia missionis & 0.877
Atalantia monophylla & 0.773
Aulacocalyx dievilleoides & 0.539
Autranella congolensis & 0.720
Auxemma gardneriana & 0.654
Auxemma oncocalyx & 0.654
Averrhoa carambola & 0.549
Avicennia africana & 0.779
Avicennia germinans & 0.661
Avicennia marina & 0.661
Avicennia nitida & 0.744
Avicennia officinalis & 0.654
Azadirachta indica & 0.690
Azadirachta spp. & 0.520
Azanza garkeana & 0.693