What is the name of the data file?
91eff.x
Do you want to read the run control cards from the file runf?
0 - no 1 - yes
0
How many rows are there in the X matrix (400 or fewer)?
16
How many columns are there in the X matrix (75 or fewer)?
12
1.0000000000000 1.0000000000000 0. 1.0000000000000 0. 0.
1.0000000000000 0. 0. 0. 0. 0.
1.0000000000000 1.0000000000000 0. 1.0000000000000 0. 0.
1.0000000000000 0. 0. 0. 0. 0.
1.0000000000000 1.0000000000000 0. 1.0000000000000 0. 0.
1.0000000000000 0. 0. 0. 0. 0.
1.0000000000000 1.0000000000000 0. 0. 1.0000000000000 0. 0.
1.0000000000000 0. 0. 0. 0.
1.0000000000000 1.0000000000000 0. 0. 1.0000000000000 0. 0.
1.0000000000000 0. 0. 0. 0.
1.0000000000000 1.0000000000000 0. 0. 0. 1.0000000000000 0. 0.
1.0000000000000 0. 0. 0.
1.0000000000000 1.0000000000000 0. 0. 0. 1.0000000000000 0. 0.
1.0000000000000 0. 0. 0.
1.0000000000000 1.0000000000000 0. 0. 0. 1.0000000000000 0. 0.
1.0000000000000 0. 0. 0.
1.0000000000000 0. 1.0000000000000 1.0000000000000 0. 0. 0. 0.
0. 1.0000000000000 0. 0.
1.0000000000000 0. 1.0000000000000 1.0000000000000 0. 0. 0. 0.
0. 1.0000000000000 0. 0.
1.0000000000000 0. 1.0000000000000 0. 1.0000000000000 0. 0. 0.
0. 0. 1.0000000000000 0.
1.0000000000000 0. 1.0000000000000 0. 1.0000000000000 0. 0. 0.
0. 0. 1.0000000000000 0.
1.0000000000000 0. 1.0000000000000 0. 1.0000000000000 0. 0. 0.
0. 0. 1.0000000000000 0.
1.0000000000000 0. 1.0000000000000 0. 0. 1.0000000000000 0. 0.
0. 0. 0. 1.0000000000000
1.0000000000000 0. 1.0000000000000 0. 0. 1.0000000000000 0. 0.
0. 0. 0. 1.0000000000000
1.0000000000000 0. 1.0000000000000 0. 0. 1.0000000000000 0. 0.
0. 0. 0. 1.0000000000000
Do you want to evaluate the design of an experiment, or
do you want to analyze the results from an experiment?
Design - 0 Analysis - 1
1
19.000000000000
20.000000000000
21.000000000000
24.000000000000
26.000000000000
22.000000000000
25.000000000000
25.000000000000
25.000000000000
27.000000000000
21.000000000000
24.000000000000
24.000000000000
31.000000000000
32.000000000000
33.000000000000
Do you wish to test the hypothesis c1'b = c2'b = ... = cq'b = 0
for some q and some c's? 0 - no 1 - yes
1
What is q?
5
What are the c primes?
0. 0. 0. 1.0000000000000 -1.0000000000000 0. 1.0000000000000
-1.0000000000000 0. 0. 0. 0.
0. 0. 0. 1.0000000000000 0. -1.0000000000000 1.0000000000000 0.
-1.0000000000000 0. 0. 0.
0. 1.0000000000000 -1.0000000000000 0. 0. 0. 1.0000000000000 0.
0. -1.0000000000000 0. 0.
0. 1.0000000000000 -1.0000000000000 1.0000000000000 -1.0000000000000
0. 1.0000000000000 0. 0. 0. -1.0000000000000 0.
0. 1.0000000000000 -1.0000000000000 1.0000000000000 0.
-1.0000000000000 1.0000000000000 0. 0. 0. 0. -1.0000000000000
The hypothesis sum of squares is 0.2389E+03
The hypothesis dof is 5
The residual sum of squares is 0.2000E+02
The residual dof is 10
The f statistic is 0.2389E+02
The p value is 0.2919E-04
Do you wish to estimate linear combinations of the parameters c1'b, c2'b, ... , cq'b
for some q and for some c's? 0 - no 1 - yes
0
Do you wish to test the hypothesis c1'b = c2'b = ... = cq'b = 0
for some q and some c's? 0 - no 1 - yes
1
What is q?
2
What are the c primes?
0. 0. 0. 0. 0. 0. 1.0000000000000 -1.0000000000000 0.
-1.0000000000000 1.0000000000000 0.
0. 0. 0. 0. 0. 0. 1.0000000000000 0. -1.0000000000000
-1.0000000000000 0. 1.0000000000000
The hypothesis sum of squares is 0.7163E+02
The hypothesis dof is 2
The residual sum of squares is 0.2000E+02
The residual dof is 10
The f statistic is 0.1791E+02
The p value is 0.4954E-03
Do you wish to estimate linear combinations of the parameters c1'b, c2'b, ... , cq'b
for some q and for some c's? 0 - no 1 - yes
0
Do you wish to test the hypothesis c1'b = c2'b = ... = cq'b = 0
for some q and some c's? 0 - no 1 - yes
1
What is q?
1
What are the c primes?
0. 0.99999900000000 -0.99999900000000 0. 0. 0. 0.33333300000000
0.33333300000000 0.33333300000000 -0.33333300000000 -0.33333300000000
-0.33333300000000
The hypothesis sum of squares is 0.6171E+02
The hypothesis dof is 1
The residual sum of squares is 0.2000E+02
The residual dof is 10
The f statistic is 0.3086E+02
The p value is 0.2424E-03
Do you wish to estimate linear combinations of the parameters c1'b, c2'b, ... , cq'b
for some q and for some c's? 0 - no 1 - yes
0
Do you wish to test the hypothesis c1'b = c2'b = ... = cq'b = 0
for some q and some c's? 0 - no 1 - yes
1
What is q?
2
What are the c primes?
0. 0. 0. 1.0000000000000 -1.0000000000000 0. 0.50000000000000
-0.50000000000000 0. 0.50000000000000 -0.50000000000000 0.
0. 0. 0. 1.0000000000000 0. -1.0000000000000 0.50000000000000 0.
-0.50000000000000 0.50000000000000 0. -0.50000000000000
The hypothesis sum of squares is 0.7717E+02
The hypothesis dof is 2
The residual sum of squares is 0.2000E+02
The residual dof is 10
The f statistic is 0.1929E+02
The p value is 0.3694E-03
Do you wish to estimate linear combinations of the parameters c1'b, c2'b, ... , cq'b
for some q and for some c's? 0 - no 1 - yes
1
Are the c's the same as those used in the hypothesis testing? 0 - no 1 - yes
0
What is q?
1
What are the c primes?
0. 0. 0. 1.0000000000000 -1.0000000000000 0. 0.50000000000000
-0.50000000000000 0. 0.50000000000000 -0.50000000000000 0.
What are the individual and the joint alphas?
(confidence level = (1 - alpha)*100 %)
5.0000000000000D-02 5.0000000000000D-02
The confidence level for the individual confidence intervals is 95.0 percent
The confidence level for the joint confidence intervals is 95.0 percent
The estimates, individual confidence intervals, and joint confidence intervals are
estimate individual joint
c 1'b -0.1000E+01 -0.3034E+01 0.1034E+01 -0.3034E+01 0.1034E+01
Do you wish to test the hypothesis c1'b = c2'b = ... = cq'b = 0
for some q and some c's? 0 - no 1 - yes
0
Do you wish to estimate linear combinations of the parameters c1'b, c2'b, ... , cq'b
for some q and for some c's? 0 - no 1 - yes
0